E309-16 Welding Electrode

1.Qualified tensile strength and hardness

2.Approved by ISO9001, CE, SGS, BV, Form-E, CO , MTC Certificates

3. Quick delivery and standard wooden exporting package.

4. Low MOQ and Flexible Production Ability.

5.Support payment with T/T, L/C , paypal, kunlun bank, etc.

6. OEM and ODM, welcome customers to visit our factory for better understanding;

7. Our factory provide steel products with competitive price and reliable quality;

8. Value friendship and trustworthy, devote to provide long-term service to our distinguished customers.

+8613222808717
+86 13222808717
Darren@screwmetal.com
Contact us

Chemical composition of deposited metal

ProjectCCrNiMoMnSiPSCu
Guaranteed value≤0.1522.0-25.012.0-14.0≤0.750.5-2.5≤1.00≤0.04≤0.03≤0.75
Example0.0624.0012.400.251.080.690.0250.0100.18


Mechanical properties of deposited metal

ProjectTension strengthRm/MPaElongationA(%)
Guaranteed value≥550≥25
Example59540


Reference current

Welding diameter(mm)Φ2.5Φ3.2Φ4.0Φ5.0
Welding length(mm)300350400400
Welding current(A)60~8585~110110~160160~200


Features:

A302 is a Cr23Ni13 stainless steel electrode with calcium titanium coating. The deposited metal has good crack resistance and oxidation resistance. It can be used for both AC and DC, and has good operating performance.


Usage:

Used for welding the same type of stainless steel, stainless steel lining, dissimilar steel (Cr19Ni10 is the same as low carbon steel), high chromium steel, high manganese steel, etc.


Precautions:

1. The electrode must be baked at about 250℃ for 1 hour before welding.

2. Rust, oil, moisture and other impurities on the weldment must be removed before welding.

3. It is recommended to use a DC power supply. The current should not be too large to avoid redness and cracking of the drug skin.

4. Reduce heat output and the swing range of the welding rod should .